HIGHLIGHTS
- What: The following key findings from the tests carried out on the physical and mechanical engineering properties, of 10, 20, 30, and 40 wt.% of treated wood flour added to the PPR matrix, are concluded:. the density increased with increasing the percentage of TWF,. the melt flow rate decreased with increasing the percentage of TWF,. the modulus of elasticity increased with increasing the percentage of TWF,. the tensile strength and strain increased with increasing TWF percentages,. the hardness increased with increasing the percentage of TWF.