HIGHLIGHTS
SUMMARY
The difference in the means was similar between the tests performed on bones decellularized with the SDS protocol and native bones for pull-out test: +1.4% (CI95% ) of mean differences when comparing Native vs D1, compression -14.9% (CI95% ), 3-point bending -5.7% (CI95% ) and indentation -10.8% (CI95% ). Mechanical evaluation of decellularized bone grafts results from those obtained with the SDS protocol or native bones during the pull-out screw +40.7% (CI95% ) for Native vs D2 protocol and 3-point bending tests +39.2% (CI95% ) for Native vs D2 protocol . . .