Visualizing the failure of solid electrolyte under gpa-level interface stress induced by lithium eruption

HIGHLIGHTS

  • who: Haowen Gao from the (UNIVERSITY) have published the article: Visualizing the failure of solid electrolyte under GPa-level interface stress induced by lithium eruption, in the Journal: (JOURNAL) of 11/03/2022
  • what: By weakening the mechanical constraint, the authors demonstrate the damage- a free Li deposition at a current density up to Au00b7cm-2 level. Such damage-free Li deposition is highly repeatable, which is also solid evidence showing that the high pressure (under a strong constraint), instead of SE defects or local current density, is the primary reason for SE damage ( the . . .

     