SUMMARY
It was found that the density and late compressive strength of MKPC mixed with fly ash and silica fume were higher than those of MKPC without fly ash and silica fume under both air and water curing. The appearance and compressive strength of MKPC after high temperatures with different fly ash and silica fume admixtures were analyzed, and the variation of the internal temperature of MKPC composite laminate with optimal ratio was evaluated with time. The test explode in the high‐temperature furnace, before the high‐temperature test, the test block explode in the high‐temperature furnace . . .