HIGHLIGHTS
- who: TECHNOLOGY and collaborators from the Department of Biomedical Engineering, National Cheng Kung University, Tainan, Taiwan, Department of Bioengineering have published the article: A Computational Pitting Corrosion Model of Magnesium Alloys, in the Journal: (JOURNAL)
- what: Autonomous models such as cellular automata (CA) techniques (Cui et_al, 2019), the finite volume method (FVM) (Scheiner and Hellmich, 2009), peridynamic (PD) formulations (Jafarzadeh et_al, 2018), and phase-field (PF) models (Tsuyuki et_al, 2018) were focused on calculating the motion of corrosion front directly. In this study, a semi-autonomous computational model based on the Monte Carlo process is . . .