A dislocation-scale characterization of the evolution of deformation microstructures around nanoindentation imprints in a tial alloy

HIGHLIGHTS

  • who: Antoine Guitton and colleagues from the Université de Lorraine, CNRS, Arts et Métiers ParisTech, LEM3, Metz, France have published the research work: A Dislocation-Scale Characterization of the Evolution of Deformation Microstructures around Nanoindentation Imprints in a TiAl Alloy, in the Journal: (JOURNAL)
  • what: The investigation presented in this Article focuses on the study of deformation mechanisms at the mesoscopic scale. With an original combination of experiments, the authors investigate the evolution of deformation microstructures at RT in the γ phase of a dual-phase bulk TiAl alloy.
  • how: In this work . . .

     