A review on atom probe and correlative microscopy studies of corrosion in nickel-based superalloys

HIGHLIGHTS

  • who: C. Rodenkirchen from the (UNIVERSITY) have published the research: A review on atom probe and correlative microscopy studies of corrosion in nickel-based superalloys, in the Journal: (JOURNAL)
  • what: They reported formation of a previously unreported, nanocrystalline phase enveloping the channels, with composition ­Na2Ni2SO5, although the transmission electron microscopy (TEM)-EDX technique used in this study has known limitations in oxygen measurement.
  • future: For more detailed characterization of smaller features on nanometer length scales however high-resolution investigation tools such as TEM and atom probe tomography (APT) are needed.6869 APT provides . . .

     