A review on pitting corrosion and environmentally assisted cracking on duplex stainless steel

HIGHLIGHTS

  • who: Menghao Liu et al. from the Institute for Advanced Material and Technology, University of Science and Technology Beijing, Beijing, China have published the research work: A review on pitting corrosion and environmentally assisted cracking on duplex stainless steel, in the Journal: (JOURNAL)
  • what: The review found that the primary reasons for the failure of duplex stainless steels are pitting corrosion and chloride-induced stress corrosion cracking. The study on the environmental response of passive films focuses on their semiconductor properties, compositions, and structural response characteristics. This research shows that manganesecontaining inclusions exhibit different dissolution . . .

     