HIGHLIGHTS

  • who: Juan Leon-Becerra and colleagues from the Research Group in Energy and Environment GIEMA, School of Mechanical Engineering, Universidad Industrial de Santander, Bucaramanga, Colombia have published the article: Comparison of Models to Predict Mechanical Properties of FR-AM Composites and a Fractographical Study, in the Journal: Polymers 2022, 14, 3546. of /2022/
  • what: Given the recent interest in their mechanical performance and failure mechanisms this work aims to describe the principal failure mechanisms and compare the prediction capabilities for the mechanical properties stiffness constants and strength of cFRAM using two distinct predictive models.
  •  