HIGHLIGHTS
- who: Mingsong Chen and colleagues from the Light Alloy Research Institute, Central South University, Changsha, China have published the article: Effect of Deformation Parameters of an Initial Aged GH4169 Superalloy on Its Microstructural Evolution during a New Two-Stage Annealing, in the Journal: Materials 2022, 15, x FOR PEER REVIEW of /2022/
- what: For the specimen deformed at the true strain of 0.36, the degree of recrystallization after AT was lower than that of the sample withcompressive the true strain of 1.20 9a,b).
SUMMARY
As a high-temperature . . .