HIGHLIGHTS
- who: Stephen Okhiai Emokpaire and colleagues from the Sciences, Shenyang, China School of Materials Science and Engineering, University of Science and Technology of China have published the Article: Effect of Ru on Deformation Mechanism and Microstructure Evolution of Single-Crystal Superalloys under Medium-Temperature and High-Stress Creep, in the Journal: Materials 2023, 16, x FOR PEER REVIEW strain. of /2023/
- what: In this work the effect of the Ru element on the u03b30 -phase evolution and deformation mechanism in the fourth-generation Ni-based single-crystal superalloy was investigated. This behavior is consistent with . . .