    In study, the mineral-PLLA composites fabricated using injection were subjected to degradation in_vitro in Hank`s balanced salts solution. Bremrer et_al used the guide of_[13] for the evaluation of the degradation in_vitro potentiality of the poly(ester)urethane-based adhesive. The profile of the in_vitro degradation of the various usable forms and compositions containing PLA differed in relation to the content and proportion of the additives. Bogdanova et_al received the 10% weight loss only during the in_vitro degradation of the electrospun PLA-gelatin composition for 8 weeks in PBS and Fenton`s solution. The application . . .

     