HIGHLIGHTS
- who: Chia-Ying Kang and collaborators from the Department of Optoelectronics and Materials Technology, National Taiwan Ocean University have published the paper: Effects of Micro-Shot Peening on the Stress Corrosion Cracking of Austenitic Stainless Steel Welds, in the Journal: Metals 2023, 13,13, 69 69 Metals 2023, of /2023/
- what: The effect of micro-shot peening on the SCC susceptibility of the SS welds is less disclosed in the open literatures; therefore, the aim of this study is to evaluate the role of micro-shot peening on the SCC behavior of the 304 and . . .