HIGHLIGHTS
- who: Zhipeng Zhang and collaborators from the Northeastern University, Shenyang, China have published the research work: Effects of Post-Weld Heat Treatment on Microstructure and Mechanical Properties of the Brazed Joint of a Novel Fourth-Generation Nickel-Based Single Crystal Superalloy, in the Journal: Materials 2023, 16, Figure x FOR PEER REVIEW 16 13. Mechanical of brazed joints of before and afterbefore the PWHT: (a) high temperature Figureproperties 13. Mechanical properties brazed joints and after the PWHT: (a) high temper of 17/Dec/2022
- what: The brazed joint is subjected to PWHT, which is the . . .