Evaluation of stress corrosion cracking of irradiated 304l stainless steel in pwr environment using heavy ion irradiation

HIGHLIGHTS

  • who: Jyoti Gupta et al. from the CEA Saclay Universit! es, Gif-sur-Yvette , France have published the Article: Evaluation of stress corrosion cracking of irradiated 304L stainless steel in PWR environment using heavy ion irradiation, in the Journal: (JOURNAL)
  • what: This study proposed that a certain amount of localized deformation is necessary to obtain Inter-Granular Stress Corrosion Cracking (IGSCC), which is related to the surface oxide film breakage either by grain boundary sliding or by the high local stresses induced locally by dislocation_channel-grain boundary interactions . The aim of this study is to . . .

     