HIGHLIGHTS
- who: Runjun He and colleagues from the AECC Beijing Institute of Aeronautical Materials, Beijing, China School of Technology, Beijing Forestry University, Beijing, China have published the Article: Experimental Study of As-Cast and Heat-Treated Single-Crystal Ni-Based Superalloy Interface Using TEM, in the Journal: Nanomaterials 2023, 608 of /2023/
- what: The authors show that property heat treatment can obviously improve the u03b3 and u03b30 lattice constant fitness and reduce the u03b3/u03b30 interface misfit. The aim of depositing a Pt layer is to reduce the Figure 2f. The main conclusions inand this dendritic . . .