HIGHLIGHTS

  • who: Maria-Alexandra Paun et al. from the School of Engineering, Swiss Federal Institute of Technology (EPFL), Lausanne, Switzerland Department of Physics, Faculty of Applied Sciences, University Politehnica of Bucharest have published the research: Fractal Analysis and Time Series Application in ZY-4 SEM Micro Fractographies Evaluation, in the Journal: (JOURNAL)
  • what: For a simple understanding, the authors provide below some classic examples such as measuring the retail sales value every day or month in a whole year, ocean tide elevations, sunspot counts on a given surface, and electrocardiograms (ECGs)-heart-activity monitoring, each being . . .

     