HIGHLIGHTS
- who: A. J. Goodfellow from the (UNIVERSITY) have published the paper: Gamma Prime Precipitate Evolution During Aging of a Model Nickel-Based Superalloy, in the Journal: (JOURNAL)
- what: EXPERIMENTAL DETAILS To characterize the effect of aging on microstructure, a model Ni-based superalloy was designed, with nominal composition given in Table I. This composition lies within the range of current, high-strength polycrystalline Ni-based superalloys, such as RR1000,[10] and is intended to have low lattice misfit between the γ matrix and γ′ precipitate phases at room temperature, comparable to certain commercial disk alloys.[11,12 . . .