- who: Yongquan Qing and collaborators from the School of Materials Science and Engineering, Northeastern University, Shenyang, China have published the paper: Impact of Atomization Pressure on the Particle Size of Nickel-Based Superalloy Powders by Numerical Simulation, in the Journal: Materials 2022, 15, 3020. of /2022/
- what: The authors report the application of computational fluid dynamics to simulate the breaking behavior of droplets in the process of preparing nickel-based superalloy powders by VIGA as well as the results on the effect of gas pressure on the atomization process and powder particle size distribution of . . .