HIGHLIGHTS
- who: Rakesh Chaudhari and colleagues from the Department of Mechanical Engineering, School of Technology, Pandit Deendayal Energy University, Gandhinagar, India have published the paper: Implementation of Passing Vehicle Search Algorithm for Optimization of WEDM Process of Nickel-Based Superalloy Waspaloy, in the Journal: Nanomaterials 2022, 12, x FOR PEER REVIEW of /2022/
- what: The analysis of variance (ANOVA) method was used to check the adequacy and suitability of the models and to understand the significance of the parameters. In the present study, machining variables (Ton, Toff, and current) along with their levels were chosen on . . .