Influence of size effect in milling of a single-crystal nickel-based superalloy

HIGHLIGHTS

  • who: Luis Soriano Gonzalez and colleagues from the University of Birmingham, Edgbaston, Birmingham , TT, UK have published the Article: Influence of Size Effect in Milling of a Single-Crystal Nickel-Based Superalloy, in the Journal: Micromachines 2023, 313 of /2023/
  • what: This work aims to investigate the influence of the size effect on chip formation, tool wear, cutting forces and surface quality when slot-milling a single-crystal Ni-based superalloy using micro- (u00d8 1 mm) and conventional/macro-sized (u00d8 4 mm) end-mills, with the results subsequently analysed to estimate the hmin value . . .

     