HIGHLIGHTS
- who: Arkadiusz Bernaczyk et al. from the Jowat SE, Detmold, Germany Department of Wood Science and Thermal Techniques, Poznanu0301 University of Life Sciences have published the paper: Investigations on the Characterization of Various Adhesive Joints by Means of Nanoindentation and Computer Tomography, in the Journal: Materials 2022, 15, x FOR PEER REVIEW As shown in Figure 5, the two methods correlate with each other. Only for one variant (EPI) the method (adhesive layer on glass) showed a very large spread. of /2022/
- what: The model was applied to beech samples joined with three different types . . .