Novel dihydro-1,3,2h-benzoxazine derived from furfurylamine: crystal structure, hirshfeld surface analysis, photophysical property, and computational study

HIGHLIGHTS

  • who: Worawat Wattanathana and colleagues from the Department of Materials Engineering, Faculty of Engineering, Kasetsart University have published the paper: Novel Dihydro-1,3,2H-benzoxazine Derived from Furfurylamine: Crystal Structure, Hirshfeld Surface Analysis, Photophysical Property, and Computational Study, in the Journal: Crystals 2021, 568 of /2021/
  • what: The authors report the synthesis of the monomer referred to as 3-(furan-2-ylmethyl)-6-methyl-3 4-dihydro-2H-benz [1 3]oxazine or (I) from a one-pot Mannich reaction using p-cresol paraformaldehyde and furfurylamine (a amine).

SUMMARY

    Dihydrobenzoxazines . . .

     