HIGHLIGHTS
- who: William Sean James from the Welding Engineering and Laser Processing Centre, Cranfield University, Cranfield, Bedfordshire , AL, UK have published the paper: Selection and performance of AM superalloys for high-speed flight environments, in the Journal: (JOURNAL)
- future: To increase the strength of the alloys further an inter-pass cold working process could be included in the WAAM process combined with a post-deposition heat-treatment which will be investigated in a future article. Research is required to establish processing methods which can return WAAM-deposited creep-resistant alloys to their wrought performance. This explains . . .

If you want to have access to all the content you need to log in!