HIGHLIGHTS
SUMMARY
This claim describes the deposition and characterization of translucent and conducting In2 O3 films that have been gadolinium oxide doped with Gd. The authors create thin film samples and powdered Gd-doped In2 O3 (dilute concentration). The polycrystalline composites (In1-x Gdx )2 O3 with x=0, 2, 4, 6, 8, and 10 at.% were created by combining analytical powders of Gd2 O3 and In2 O3 (Sigma-Aldrich purity 99.998%) using the following equation: (Gd2 O3 ) + (1 - x) In2 O3 → (In1-x Gdx )2 O3 At ambient temperatures, all Gd-doped In2 O3 . . .