HIGHLIGHTS
- who: Bou017cena Szczucka-Lasota et al. from the Faculty of Transport and Aviation Engineering, Silesian University of Technology, Krasinu0301skiego, Katowice, Poland have published the article: Superalloyu2014Steel Joint in Microstructural and Mechanical Characterisation for Manufacturing Rotor Components, in the Journal: Materials 2023, 16, x FOR PEER REVIEW of 24/03/2023
- what: The analysis of the literature and published patents in the field of joining difficult-toweld nickel alloys with steels clearly shows the lack of guidelines for the welding process and the use of relatively simple methods to obtain correct welds, which can be considered . . .