Surface analysis of ti-alloy micro-grooved 12/14 tapers assembled to non-sleeved and sleeved ceramic heads:a comparative study of retrieved hip prostheses

HIGHLIGHTS

  • who: Andrea Martelli et al. from the Laboratorio Tecnologia Medica, IRCCS Istituto Ortopedico Rizzoli, Bologna, Italy have published the paper: Surface Analysis of Ti-Alloy Micro-Grooved 12/14 Tapers Assembled to Non-Sleeved and Sleeved Ceramic Heads:A Comparative Study of Retrieved Hip Prostheses, in the Journal: Materials 2023, 16, 1067. of /2023/
  • what: This study evaluated both qualitatively and quantitatively the damage that occurred in vivo on Ti-alloy 12/14 of_(i) primary implants with (Group 1) (ii) secondary implants with (Group 2) and_(iii) secondary implants with (Group 3). total of . . .

     