SUMMARY

    Of 20 There are several ways to make WC powder including heating tungsten-carbon mixtures in carbon tubes to temperatures of 2800 ◦ C in microwave ovens or interacting them with hydrogen, methane, and vacuum at temperatures of 1400-2000 ◦ C. In this work, a systematic parametric study was performed on the synthesis of WC, TiC, and WC-TiC powders by the means of high-temperature synthesis and mechanochemical synthesis. It has been demonstrated that (W,Ti)C powder can be produced using mechanochemical synthesis, however, further research needs to be conducted to determine the . . .

     