The effect of tic–tib2 dual-phase nanoparticles on the microstructure and mechanical properties of cast ni–fe-based superalloys

HIGHLIGHTS

  • What: This study provides valuable insights for selecting ceramic nanoparticles to increase the mechanical properties of cast
  • Who: Guanlan Liu and colleagues from the Jilin University, No, Renmin Street, Changchun, China have published the research: The Effect of TiC-TiB2 Dual-Phase Nanoparticles on the Microstructure and Mechanical Properties of Cast Ni-Fe-Based Superalloys, in the Journal: Materials 2024, 17, 5781. of /2024/

SUMMARY

    The experiment demonstrated the semi-coherence of the interface between TiC and Ni matrix, and the orientation relationship was TiC //(1(_)1(_)1(_ . . .

     