Effect of overheating on the tensile properties of nickel-based superalloy gh4720li

HIGHLIGHTS

  • What: In this work, OEI conditions were determined based on the actual O using an MTS Model 809 hydraulic testing machine to evaluate the alloy`s tensile properties a specific typestrength of aero-engine.
  • Who: Anqi Wang and collaborators from the College of Mechanical and Vehicle Engineering, Hunan University, Changsha, China have published the paper: Effect of Overheating on the Tensile Properties of Nickel-Based Superalloy GH4720Li, in the Journal: Materials 2024, 2351 of /2024/
  • How: The results showed that after OEI treatment the primary γ′ phase in this alloy was partially dissolved.
  •  